STYRENE BUTADEINE RUBBER
SBR 1502
PARAMETER | TEST METHOD | UNIT | VALUE |
Volatile Matter | ASTM D1416 | %wt | 0.75 max |
Ash | ASTM D1416 | %wt | 1.5 max |
Organic Acid | ASTM D416 | %wt | 4.75-7 |
Soap | ASTM D1416 | %wt | 0.5 max |
Bound Styrene | ASTM D1416 | %wt | 22.5-24.5 |
Raw Viscosity (ML 1+4 @ 100°C) | ASTM D1646 | – | 46-58 |
Compound Viscosity (ML 1+4 @ 100°C) | ASTM D1646 | – | 84 max |
tensile Strength (35 Minutes Cure) | ASTM D412 | kg/cm2 | 250 min |
Ultimate Elongation (35 Minutes Cure) | ASTM D412 | % | 350 min |
300% Modulus (35 Minutes Cure) | ASTM D412 | kg/cm2 | 167-207 |
Volatile Matter | ASTM D1416 | %wt | 0.75 max |
APPLICATIONS
Shoes industries, bicycle tires, toy, tire,mechanical & cable industries