POLYPROPYLENE COPOLYMER
EXTRUSION GRADE

PPCP EP-S 31 HP

PARAMETERTEST METHODVALUEUNIT
Melt flow rate (230 °C, 2.16 kg)ISO 11331.3dg / min
DensityISO 11830.9g/cm3  
Flexural modulusISO 1781350N/mm2
Tensile strength yieldISO R 52727N/mm2
Elongation at yieldISO R 5278%
Izod Impact Strength (notched) at 23°CISO 18040kJ/m2
Hardness Shore DISO 86868Points
Vicat softening point (9.8 N)ISO 306/A152°C
H.D.T. (0.46 Mpa)ISO 75/B100°C
Accelerated oven ageing in air

(forced circulation) at 150 °C

ISO 4577360hours
APPLICATIONS

Conduit pipes and fittings for electrical distribution and cable protection, Corrugated pipes for automobile and machine construction, plane- and shipbuilding and for domestic appliances, extrusion blow molding of bottles and containers and for the extrusion of corrugated board